Dear All,

I'm from Hungary.
Under my work I met the next material : A5052W-H32.
This is some Carbon steel, according to the JIS G 3539 japanese standard.
I need some similar material to subsitute, wich is procurable in EU. (according DIN or ISO standards)
I'll be very grateful if you can help me.

Thanks
Gagar
 
Replies continue below

Recommended for you

Sorry, I made a mistake. This is not according to the JIS G 3539 standard. This material is an aluminium or aluminium alloy (JIS H 4040).

The question is the same.

Thanks
Gagar
 
Hi Gagar,

A5052 is a very common aluminum alloy composition, which is essentially the same as Al 5052, UNS A95052, EN AW 5052 and ISO (DIN) AlMg2,5 [in the EN spec., 'AW' indicates Aluminum, Wrought]. See more alloy cross-listings at
H32 is the temper. In this case, the aluminum has been strain hardened (cold worked) and then given a stabilizing heat treatment (at 120-175oC), which gives a final hardness 1/4 between the annealed and maximum cold worked conditions.

'w' may indicate that the product form is wire. I don't have the Japanese standards, only their titles, but I note that the applicable specification is
JIS H 4040:1999 Aluminum and aluminum alloy, bars and wires.
whereas other JIS H 40xx & 41xx standards are for other forms. E.g.,

JIS H 4000:1999 Aluminum and aluminum alloy, strips and coiled sheets
JIS H 4100:1999 Aluminum and aluminum extruded shape
JIS H 4140:1988 Aluminum and aluminum alloy forged part

A Budapest producer of A5052 wire:
 
Thank you very much!

Huhh, it was so detailed..

 