Does anyone know where I can find corrosion rates for A36 steel in a severe marine environment?

I have crevice corrosion between a clevis and gusset plate less than 1/4 mile from the ocean.

Thanks,
Nick
 
Replies continue below

Recommended for you

There are various sources for this information and it will depend on several factors - besides distance from the ocean, pollution (industrial)and location, location and location will effect the rate.

From ASM Handbook, Volume 13C

the rate of low carbon steel (similar to A 36) in a marine environment can vary from 0.53 mils/yr (rural) to 3.57 mils/yr (industrial), 5.73 mils/yr(mild) to 20 mils/yr (severe).
 