Jan 10, 2005 #1 reichertc Mechanical Joined Mar 21, 2001 Messages 115 Location CA I'm trying to find out what the 1997 version of ASTM A350 says regarding the LF2 material. 1996 does not specify different classes, the 1999 version specifies Class 1 and Class 2. Does 1997 specify different classes? (Cross Posted under ASTM)
I'm trying to find out what the 1997 version of ASTM A350 says regarding the LF2 material. 1996 does not specify different classes, the 1999 version specifies Class 1 and Class 2. Does 1997 specify different classes? (Cross Posted under ASTM)
Jan 11, 2005 #2 codeeng Petroleum Joined Feb 9, 2004 Messages 365 Location CA I have a 98 edition which does not cover Class 1 or 2 and a 2001 edition that does. Upvote 0 Downvote