Jan 7, 2005 #1 oneandonly Mechanical Joined Jan 7, 2005 Messages 1 Location US Have a stud made with ASTM A320-L7. What is the ultimate strength of this material?
Jan 7, 2005 1 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Per SA 320; Grade L7 (2.5" and under in diameter) UTS - 125 Ksi min Upvote 0 Downvote