Mar 9, 2016 #1 pflow Mechanical Joined Jan 25, 2008 Messages 52 Location US I have been searching to no avail for the difference between A312 TP304 and A312 13b TP304. Any information would be appreciated.
I have been searching to no avail for the difference between A312 TP304 and A312 13b TP304. Any information would be appreciated.
Mar 10, 2016 #2 XL83NL Mechanical Joined Mar 3, 2011 Messages 3,122 Location NL Im not exactly sure what 13b means, but it seems to refer to a certain edition of A312. Is that what your question is about? If so, then Im not sure to which (other) edition you're comparing it. Upvote 0 Downvote
Im not exactly sure what 13b means, but it seems to refer to a certain edition of A312. Is that what your question is about? If so, then Im not sure to which (other) edition you're comparing it.
Mar 10, 2016 #3 DVWE Petroleum Joined Apr 5, 2007 Messages 2,380 Location US It appears that in 2013, A312 was revised twice. There was initial release, rev A and rev B. I believe that's what the 13b is referring to. Upvote 0 Downvote
It appears that in 2013, A312 was revised twice. There was initial release, rev A and rev B. I believe that's what the 13b is referring to.
Mar 10, 2016 #4 bimr Civil/Environmental Joined Feb 25, 2003 Messages 9,388 Location US ASTM A312/A312M - 16 is the current standard. Publication Date 01 January 2016. Document History is: ASTM A312/A312M STCH 2015-11-01 15B INAC ASTM A312/A312M STCH 2015-09-01 15A INAC ASTM A312/A312M STCH 2015-03-01 15 INAC ASTM A312/A312M STCH 2014-11-01 14B INAC ASTM A312/A312M STCH 2014-10-01 14A INAC ASTM A312/A312M STCH 2014-03-01 14 INAC ASTM A312/A312M STCH 2013-10-01 13B INAC A Summary of Changes section appears at the end of the standard. You would have to purchase 8 of these standards for the paper trail: http://standards.globalspec.com/std/9970123/astm-a312-a312m Upvote 0 Downvote
ASTM A312/A312M - 16 is the current standard. Publication Date 01 January 2016. Document History is: ASTM A312/A312M STCH 2015-11-01 15B INAC ASTM A312/A312M STCH 2015-09-01 15A INAC ASTM A312/A312M STCH 2015-03-01 15 INAC ASTM A312/A312M STCH 2014-11-01 14B INAC ASTM A312/A312M STCH 2014-10-01 14A INAC ASTM A312/A312M STCH 2014-03-01 14 INAC ASTM A312/A312M STCH 2013-10-01 13B INAC A Summary of Changes section appears at the end of the standard. You would have to purchase 8 of these standards for the paper trail: http://standards.globalspec.com/std/9970123/astm-a312-a312m
Mar 10, 2016 Thread starter #5 pflow Mechanical Joined Jan 25, 2008 Messages 52 Location US Thank you everyone for taking the time to reply. That is what I needed. Upvote 0 Downvote