I have been searching to no avail for the difference between A312 TP304 and A312 13b TP304.

Any information would be appreciated.
 
Replies continue below

Recommended for you

Im not exactly sure what 13b means, but it seems to refer to a certain edition of A312.
Is that what your question is about? If so, then Im not sure to which (other) edition you're comparing it.
 
It appears that in 2013, A312 was revised twice. There was initial release, rev A and rev B.

I believe that's what the 13b is referring to.
 
ASTM A312/A312M - 16 is the current standard. Publication Date 01 January 2016.

Document History is:
ASTM A312/A312M STCH 2015-11-01 15B INAC
ASTM A312/A312M STCH 2015-09-01 15A INAC
ASTM A312/A312M STCH 2015-03-01 15 INAC
ASTM A312/A312M STCH 2014-11-01 14B INAC
ASTM A312/A312M STCH 2014-10-01 14A INAC
ASTM A312/A312M STCH 2014-03-01 14 INAC
ASTM A312/A312M STCH 2013-10-01 13B INAC

A Summary of Changes section appears at the end of the standard.

You would have to purchase 8 of these standards for the paper trail:

 
Thank you everyone for taking the time to reply. That is what I needed.
 