A193 B16 Stud Bolts size 1" produced from 23.23mm size rod

Status
Not open for further replies.

ZAbbas101054

Materials
Joined
May 18, 2014
Messages
6
Location
SA
Sir,

Could some one explain how the stud bolt size 1" be produced from 23.23mm size round bar i.e slightly greater size be produced from smaller size material.

Thanking in advance.
 
Rolled threads?

Regards,

Mike
 
The thread rolling process uses a blank at pitch diameter to make the final part with the thread major diameter larger and the minor diameter smaller than the original blank diameter.
 
Experts,

Thanking you all on your precious replies.
 