Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

A11 in ABD matrix based on CLT compared with E11 (modulus of elasticity) composite in 11 direction

Status
Not open for further replies.

Arissa

Mechanical
Joined
Sep 25, 2012
Messages
5
Location
MY
Hi there
Good day

i have some inquiry and curiosity, may I know, is the terminology/notation for A11 calculated based on CLT for homogenous composite
similar with E11? (modulus of elasticity in 11 direction)

thanks
 
Similar but not exactly the same.

E11 = 1/(a11*t) where a is from inverse of ABD
 
Many thanks SWComposites..I really appreciate your respond and reply
hence E11 is A11 divided by thickness of the laminate then?
am i right?
many thanks SWcomposites
 
Arrisa, no. To further extend:

Symmetric laminate (need not be balanced): Ex = 1/(a11*t)
Symmetric and balanced laminate: Ex = (A11-A12^2/A22)/t
Unsymmetric laminate: Calculation based upon what curvatures are restrained and only equal to the above if all curvatures are not restrained. But that is not the typical scenario and usually one or more curvature directions are suppressed when an in-plane load is applied to an unsymmetric laminate.

Brian
 
E11 in my case is E longitudinal direction
Ex = E22 right?
hence in my case E11 = Eyy
 
No.

E1 = lamina fiber or warp dirction
Ex = laminate x direction (x is usually set = 0 fiber direction)

Please get a laminated plate theory text and study it.
 
tq so much SWComposite and ESPcomposite
 