A105/LF2 ENP for non-corrosive service

Status
Not open for further replies.

MaxCarb

Mechanical
May 1, 2008
16
My Client gave me a datasheet of a ball valve, in which an electroless nickel plating surface treatment (min. thk. 50 microns)is required for a standard (non corrosive) service.
I really don't understand the advantages of this choice versus the cost of this treatment (i have 16" valves!!).

Thanks
 
Replies continue below

Recommended for you

Your customer didn't provide the working condition?
In my opinion, LF2 is carbon steel, always do phosphitized for rust prevention, maybe the medium can't allow P or something else. So do the nickel coating.
forget it. I think you just need ask the customer for the working condition directly.
 