I have a piece of steel in the shape of the disk. 10" diameter .25" thick. I need to drill 7/64's holes into the side of the disk. I punched indentions where I needed. The holes I drilled on the flat side of the steel worked fine. However as soon as I tried the curved side holes, I had a problem.
The drill bit will not engage. It simply rides on the surface.
I tried a drill press at each speed and then tried a hand drill. I used cutting oil.
Is there any way to make the drill bit go in?
The drill bit will not engage. It simply rides on the surface.
I tried a drill press at each speed and then tried a hand drill. I used cutting oil.
Is there any way to make the drill bit go in?