Im taking a quick glance at the heat loss through an insulated pipe (A-672 Gr60). I however do not have the ASTM Spec at this time. Can anyone tell me the thermal conductivity of such material @ 75F. Thanks
 
The spec ASME SA 672 does not provide heat transfer properties of the carbon steel pipe. Just try google "Wrought Carbon Steel thermal conductivity" and pick an answer. You could also generate your own graph from the answers found.
cheers,
gr2vessels
 
From ASME Section II, Part D Physical Properties Table gfor this group of steel

at 70 deg F, 12.8 BTU/hr-ft-degF
 
Thanks,
I think you meant Table TCD. But anyhow, This is exactly what I was looking for. I didnt even realize this table was in ASME Section II.
 
I think metengr may have accidently quoted the value for 9 Cr material. For carbon steel at 75°F, ASME lists the thermal conductivity as being 34.9 BTU/hr-ft-°F.

I would advise you to download 3EPlus to run these calculations: