Dear Coleagues,
We have a consult from a Refinery previewing a De-cocking procedure. Their systems are design for about 480 C. The basic material is A 335 grade P5. The De-cocking operation is arround 710C operation - 745 C design.
This is far beyond the temperature tabulated in ASME B31.3 allowable stress. According to that the maximum temperature for that material is 650 C.
The operation will last 10 hours.
Does anybody knows some paragraph or statament on B31.3 which could allow this use?
Regards,
Hansito
We have a consult from a Refinery previewing a De-cocking procedure. Their systems are design for about 480 C. The basic material is A 335 grade P5. The De-cocking operation is arround 710C operation - 745 C design.
This is far beyond the temperature tabulated in ASME B31.3 allowable stress. According to that the maximum temperature for that material is 650 C.
The operation will last 10 hours.
Does anybody knows some paragraph or statament on B31.3 which could allow this use?
Regards,
Hansito