Is the 95-5 a cleaner shielding gas as well as an aid to penetration?? I am welding 300 series SS to each other. GTAW, .060 wall. Where can I find onfo that educates me on these variables??
boo1 - Yes hydrogen is flammable. It is acceptable as part of a mix with argon for austenitic materials. Definitley not acceptable on its own, or in any quanitity when used with ferritic materials.
As torch gas or sheild gas?
We use 95/5 in plasma torches. It is hard to use as a shield gas becuase is has better thermal conductivity and my reduce penetration, but yes, it is cleaner.
5% H2 is not a saftey issue. You are below the flamability limits, and by the time you add enough air to have some O2 you are even lower.
= = = = = = = = = = = = = = = = = = = =