Jul 31, 2019 #1 Dobe Mechanical Joined Oct 1, 2003 Messages 51 Location US Can I stress relieve 50YF SAE 1392 and hold the hardness? Print is asking for Core hardness Rockwell B77 MIN. If so at what temp, how long? We also melonite after forming.
Can I stress relieve 50YF SAE 1392 and hold the hardness? Print is asking for Core hardness Rockwell B77 MIN. If so at what temp, how long? We also melonite after forming.
Jul 31, 2019 #2 Guest Please do not cross-post. "Everyone is entitled to their own opinions, but they are not entitled to their own facts." Upvote 0 Downvote
Please do not cross-post. "Everyone is entitled to their own opinions, but they are not entitled to their own facts."