Does anyone know what 4571 steel is? It PMI's as 316L, but I can't find a listing for 4571.
thanks,
 
In looking a little further it appears this may be 1.4571 which equates to 316Ti. If anybody has any other comments I'd appreciate them.
 
Here's a thread awhile back on 316Ti: