We have the choice of machining a 60 inch diameter ring from a 4340 or A106 forged ring.
The forging house will deliver the ring stress relieved and normalized.
The ring will be cut into 6 identical segments after machining.
We are considering a second thermal stress relief after rough machining to reduce ( eliminate!) distortion/spring after cutting.
Is either material likely to offer better stability to reduce distortion after cutting?
Thanks,
Dan T
The forging house will deliver the ring stress relieved and normalized.
The ring will be cut into 6 identical segments after machining.
We are considering a second thermal stress relief after rough machining to reduce ( eliminate!) distortion/spring after cutting.
Is either material likely to offer better stability to reduce distortion after cutting?
Thanks,
Dan T