Anyone has an idea why ASTM A276 "Standard specification for Stainless Steel Bars and Shapes" doesnot include the mechanical requirements for 420, 431, and 440, while all other grades, including 403, 410 martenstic grades list the strength requirements (refer to Table 2)? Thanks!
 
Replies continue below

Recommended for you

Ben, did you look on the next page at the continuation of the table 2?

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
Ed, yes this is a long table, which lists tens of grades including austenitic, austenitic-ferritic, ferritic, and martensitic grades, but only part of martensitic grades, 420,431, 440 do not include tension property requirements (tensile, yield, elongation)?!
Table_2_njxe39.jpg
 
Then the only requirement is a hardness, there is no strength required.
Some of these alloys have nil ductility, so that might be the issue.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
Send an Inquiry into ASTM committee responsible for this specification. They will get back to you with the best response.
 