I am trying to find out if anyone know how 430F or 430FR is manufactured.

Is it CAST or SINTERed process?

I wanted to make a part that will go in a vacuum environment.

Thank you.
 
Replies continue below

Recommended for you

Thank you, I will check out the links
 
I have only ever seen them as wrought products, though PM is possible but more expensive.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
I have a naive question, are P/M or cast parts recommended for vacuum application?

_____________________________________
"The richer we have become materially, the poorer we have become morally and spiritually." Martin Luther King Jr
 
usually not unless they have been vacuum impregnated with a resin. Outgassing is a big issue.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
thank you for all the replies.
Your right Ed, that is the concern here, outgassing.
 