Is chemical specification of 330 Stainless Steel and UNS N08330 (Alloy Fe-Ni-Cr-Si) same

Thanks
 
Replies continue below

Recommended for you

yes.
UNS N08330: .08 C 2.00 Mn .04 P .03 S .75-1.5 Si 17-20 Cr 34-37 Ni .1 Ta .2Cb
 
As a heat resistant steel casting follow ASTM A 297 Gr HT .