MY SPECIFICATION CALLS FOR CF-8M(316SS) WITH TS OF 75,000 YS 30,000 ENLOGATION OF 40%.
WE ARE CHANGING TO BAR STOCK DUE TO COST AND QUANTIY NEEDED SUPPLIER CERTS ARE CALLING OUT 316/316L WITH MECHANICAL PROPERTIES RUNNNING WITH IN THE GUIDELINES. IS THEIR ANY HIDDEN ISSUES WITH 316 VERSES 316L OR THE "DUAL CERTIFIED" 316/316L MATERIAL? THE CORROSION FACTOR ISN'T AN ISSUE WITH THE APPLICATION.
WHAT WILL THE LESS CARBON OF 316L BRING TO THE TABLE?
WE ARE CHANGING TO BAR STOCK DUE TO COST AND QUANTIY NEEDED SUPPLIER CERTS ARE CALLING OUT 316/316L WITH MECHANICAL PROPERTIES RUNNNING WITH IN THE GUIDELINES. IS THEIR ANY HIDDEN ISSUES WITH 316 VERSES 316L OR THE "DUAL CERTIFIED" 316/316L MATERIAL? THE CORROSION FACTOR ISN'T AN ISSUE WITH THE APPLICATION.
WHAT WILL THE LESS CARBON OF 316L BRING TO THE TABLE?