Hello all
Background:
In a 25 MM thick Carbon Steel plate(SA 516 Gr 60), 3mm SA 240 Gr 31254 is clad (Explosion Bonded).
This is rolled into a 1800 mm (ID) Shell for a Pressure vessel (U stamped vessel).
The Longitudinal seam is first welded (carbon Steel welding done with 7018-1, MDMT -29 Deg C, No Production coupon, No Impact). Subsequently 31254 is to be restored.
Nozzles are planned to be overlayed (Lowest size of nozzle is 4").
Expected Undiluted chemistry of 2mm (31254)
Question is
1) Can is use Barrier layer as Inconel (As suggested in ASME II C) and final layer with 31254 Wire? ASME or AWS suggests Inconel filler.
I am unable to find a 31254 filler wire (when i did a search, i could not find 31254 filler wire).
2) For Nozzles ID deposition (Planned with GTAW), here again if i perform barrier with Inconel (Er Ni Cr Mo-3 or Er Ni Cr Mo-12) and subsequently with 31254 Wire, is it OK?
Of course i will conduct PQR as per ASME.
The reason for this question is that, Neither ASME/AWS specifies 31254 filler nor does the manufacturer brouchers for SMO 254 (et al) specify 31254 filler wire.
3) The larger question: Suppose for another vessel/Exchanger where there is a pressure butt joint between 31254 Nozzle pipe and nozzle flange,
Can you simply procure a specified alloy wire (Not necessarily classified as filler wire) and use it as a filler wire for weld deposit?
Background:
In a 25 MM thick Carbon Steel plate(SA 516 Gr 60), 3mm SA 240 Gr 31254 is clad (Explosion Bonded).
This is rolled into a 1800 mm (ID) Shell for a Pressure vessel (U stamped vessel).
The Longitudinal seam is first welded (carbon Steel welding done with 7018-1, MDMT -29 Deg C, No Production coupon, No Impact). Subsequently 31254 is to be restored.
Nozzles are planned to be overlayed (Lowest size of nozzle is 4").
Expected Undiluted chemistry of 2mm (31254)
Question is
1) Can is use Barrier layer as Inconel (As suggested in ASME II C) and final layer with 31254 Wire? ASME or AWS suggests Inconel filler.
I am unable to find a 31254 filler wire (when i did a search, i could not find 31254 filler wire).
2) For Nozzles ID deposition (Planned with GTAW), here again if i perform barrier with Inconel (Er Ni Cr Mo-3 or Er Ni Cr Mo-12) and subsequently with 31254 Wire, is it OK?
Of course i will conduct PQR as per ASME.
The reason for this question is that, Neither ASME/AWS specifies 31254 filler nor does the manufacturer brouchers for SMO 254 (et al) specify 31254 filler wire.
3) The larger question: Suppose for another vessel/Exchanger where there is a pressure butt joint between 31254 Nozzle pipe and nozzle flange,
Can you simply procure a specified alloy wire (Not necessarily classified as filler wire) and use it as a filler wire for weld deposit?