I'm putting together a pump skid that will be used to circulate chemical cleaning solutions for boiler/HRSG chemical cleaning operations. Some of the chemistry is acidic (Citric, EDTA..) some is alkaline (Ammonia, Soda Ash...). Pumping pressures never exceed 150-160 psig and temps never exceed 180F. I'm going to use Sch10 stainless pipe with carbon steel slip-on flanges (so that wetted surface only is stainless). In selecting the stainless material, I was looking at 304L or 316L. I don't want corrosion problems around the weld areas, and I need to make an economical selection while selecting the properly suited material. Any thoughts.....? (gittings such as ells, tees, and reducers will also come into play).
Thanks,
CW3
Thanks,