Hello All
Where can i get the allowable stress for A 193 B7M (3" dia). ASME Sec II D gives allowable stress only upto 2.5" diameter.
The application: Sub Sea Flange (Sub Sea Fastener)
Where can i get the allowable stress for A 193 B7M (3" dia). ASME Sec II D gives allowable stress only upto 2.5" diameter.