As concern the materials A 266 Cl.1 and A 350 LF1 , you are kindly asked if according to ASME Code there are particular requirements for two times Post Weld Heat Treated materials.
Thank you for cooperation.
 
Replies continue below

Recommended for you

The weld procedure qualification record (WPQR) should reflect the total or cumulative time for PWHT.
 
Please refer to ASME VIII, Div.1 UCS-85, UHT-81 & UHT-82 with regard to heat treatment requirements for base materials.

 