We are looking to install a new 250mm Pipe run for Mains Water into our factory .Most of which will be underground.
The parts which are above ground we were going to spec 254 x 2mm 316 stainless steel pipe and below ground use the same pipe but wrap with Petroleum tape (denso Tape).
The other alternative would be to use plastic underground and only when it exits above ground into factory use stainless . If so what plastic would be acceptable and would it need to be Glass Lined as someone else mentioned it might need to be ?
Are there any inherent problems with using stainless steel underground ? . We would make sure there is minimum cover above pipe of 900mm & pipe bed on pea gravel or similar .The entire system will need to be pressure tested to 4 bar and chlorinated before use .
Thanks in advance for any help
Bit new to this game but want to make sure the contractors install the correct system.
We are looking to install a new 250mm Pipe run for Mains Water into our factory .Most of which will be underground.
The parts which are above ground we were going to spec 254 x 2mm 316 stainless steel pipe and below ground use the same pipe but wrap with Petroleum tape (denso Tape).
The other alternative would be to use plastic underground and only when it exits above ground into factory use stainless . If so what plastic would be acceptable and would it need to be Glass Lined as someone else mentioned it might need to be ?
Are there any inherent problems with using stainless steel underground ? . We would make sure there is minimum cover above pipe of 900mm & pipe bed on pea gravel or similar .The entire system will need to be pressure tested to 4 bar and chlorinated before use .
Thanks in advance for any help
Bit new to this game but want to make sure the contractors install the correct system.