I can not find an allowable Compressive Stress for 2101 Duplex. Does any one know where I can find this information?
 
Replies continue below

Recommended for you

Under what code? Anyway its most likely the same as the tensile as it a ductile metal and their properties as symmetrical in tensile and compressive
 