I am looking for a source of hollow bar or extruded
tube in 17-4 ph per AMS 5622
sizes
8.858" od x 6.417" id x 70 ft
13.150" od x 7.007" id x 1ft
 
Replies continue below

Recommended for you

Where are you?
I'm in North America, and I use EM Jorgensen for steel orders, and Integris for aluminum. EMJ carries 17-4, but in imperial sizes only (I see your numbers are just converted from metric). Find a food/chemical processing company or a petrochemical extraction business, those industries use lots of stainless grades.


STF
 
In North America, Plymouth Tube supplies 17-4 tubes. You can learn more at:



Regards,

Cory