Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations The Obturator on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

16B26 Steel Beam? 1

Status
Not open for further replies.

vmirat

Structural
Apr 4, 2002
294
I have a building that was built around 1971 which has 16B26 wide flange roof beams. Anyone have material properties on this shape?
 
Replies continue below

Recommended for you

What you have is a design or fabrication piece mark. This would typically designate a W16x26, a standard shape available then and now. You should be able to find the properties from a variety of sources.
 
vmirat,

16B26 was the designation of a light beam in use around the 70's. His section properties are very similar to the W16X26.

An old Bethlehem booklet show the following properties:

Area = 7.65 in^2
Depth = 15.65"
Flange width = 5.500"
Flange ave. thickness = 0.345"
web thickness = 0.250"
d/Af = 8.25
Ix = 298.1 in^4
Sx = 38.1 in^3
rx = 6.24"
Iy = 8.71 in^4
Sy = 3.17 in^3
ry = 1.07"

This section is non-compact for ASTM A242, A440 and A441 steels.