Anyone have an equivalent grade for 13CrMoV9? What is the difference for 13CrMoV9-10?

Thanks in advance.
 
Replies continue below

Recommended for you

One reference I have has SA 542 Type D Class 4a is equivalent to 13CrMoV9-10 (EN 10028-2).