Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations KootK on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

10.9 vs 8.8 Grade Bolts

Status
Not open for further replies.

danicortes22

Mechanical
Apr 1, 2019
1
What is the difference between 8.8 and 10.9 grade steel? Which one performs better under cold weather? Is there something I can reference?

Thank you,
 
Replies continue below

Recommended for you

What is the application? what is cold weather temp?
10.9 is more stronger
Cold weather will shrink both the bolt&nuts and the components attaching, if you ONLY worry about loosening consider using spring/lock washers.

see the chart from Mc Master

 
 https://files.engineering.com/getfile.aspx?folder=648e13a7-bccf-477e-a68b-11b5b2d00a1d&file=b01-aboutcapscrewsl1-gis.png
The first digit is the ultimate strength of the material and the second is the ratio of yield stress to ultimate strength. Grade 8.8 bolts have an ultimate strength of around 800 N/mm2 (MPa) and a ratio of yield/proof stress to a yield strength of 80% i.e, 640 N/mm2 (MPa).

Extreme cold weather would require special bolts, I guess.



Muthu
 
Not sure what you mean by "low temperature" but ASTM A320 (iirc) is for low temps, I used that once working a LOX system
 