we have to weld we have to weld 1" pipe with notch toughness procedure.
i do have welding procedure up to 3/4" weld.
can i used two welders with this procedures to weld 1" thick.
i do have welding procedure up to 3/4"thickness weld.
can i used two welders with this procedures to weld 1" thick pipe.
so first welder can weld 0.5" thick both side & other welder can weld remaining 0.5"weld.
please advice
stanly
i do have welding procedure up to 3/4" weld.
can i used two welders with this procedures to weld 1" thick.
i do have welding procedure up to 3/4"thickness weld.
can i used two welders with this procedures to weld 1" thick pipe.
so first welder can weld 0.5" thick both side & other welder can weld remaining 0.5"weld.
please advice
stanly