Ok so the 4mm I think is the leg length
The 5.4 bar is total pressure in the system.
The total length is actually 400mm with a nozzle at either end the baffle plate is in the middle.
There will be a gap between the round plate (baffle) and the pipe of 6mm except for the 3 weld tabs.
Its a baffle plate. Liquid will flow down between gaps around the edge and it will be weld at the 3 tabs. I don't have any flexibility in terms of actually design just need to confirm if the double 4mm fillet weld at each tab will be strong enough.
The material is SS NAG 18/10L
Shoe
Right I have been thrown in at the deep end with weld calcs. Previously I have never dealt with them so could do with some help.
I am trying to calculate if my fillet weld is going to be strong enough.
I have a circular 6mm plate, diameter =144mm that is going to be weld inside a pipe. It will...