For those of you who are familiar with the Inlet quench of smelter's sulfuric acid plant, as you may expect, we are experiencing corrosion problem on this equipment...
The inlet quench is the area where hot SO2 (300 C) gas coming from Nickel or Copper smelter is quenched by weak acid spraying...