Does anyone know why API 620 is so much more conservative on their joint design then AISC ASD?
For 38W material a single lap weld would have an allowable stress of:
API 620
S_allowable = 16,500psi x 0.35 = 5,775 psi
AISC (table J2.5)
S-allowable = 60,000psi x 0.3 x 0.707 = 12,726 psi