cold forming the ring from a rod. The thickness of the ring is 0.35 inches.
Is there any alternative to cold forming?
Can 31 RC can be acheived after the Machinig operation?
Thanks Israelkk,
How a hardness of 31 RC can be acheived? If it is not heat treatable? The cold working might be helpful but i beleive the cold work is possible with the rod before machining.
Hello All,
I have a Ring made of SS 304. The minimum hardness requires to be 31 HRC. Please advice on the heat treatment procedure.
We have trid two HT procedure as below:-
1) Heat up to 750 for 20-30 minutes and let it air cool.
2) heat up to 1250 for 30 minutes and water quech...