After spaying a base coat of a 70 Shore crosslinked PU dispersion, allowing it to dry and embossed it @ 90°C and 150 Kg, we couldn't get an even spraying of subsecuent coats of some other PU's dispersions.<br>
<br>
We have tried penetrators, tensoactives, soaps, solvents like IPA and...