  1. MATe10

    Steam Injection Line MI Thermocouple Failure

    Hello All, I have a 1/8" diameter 316 SS sheathed magnesium oxide insulted thermocouple that was placed inside a steam injection well for a SAGD operation that has failed. It was subject to ~240C temps and 1400kPa pressures and also inadvertently exposed to around 10ppm chlorides and 51 ppm...
  2. MATe10

    Welding P-7 materials to P-3, P-4, P-5A, P-1

    Does anyone have any experience welding these combinations? I was thinking ER309L but it seems like a preheat of 300F would make this filler flow way too much. ERNiCrMo-3 would give me an unacceptable hardness, I think. Any sugestions? THANKS