Ladies and Gentlmen
submersed pump for pumping liquid sulfur was failed due to corrosion, failure was in steam jacketing tube which designed to heat sulfur inside the pump, corrosion is external, material of tube is 316SS, temperature between 130 and 150C
liquid sulfur pit is air vetilated, and...
Ladies and Gentlmen
we have corrosion problem with pump used for treated water in industrial area
material of wet pump is carbon steel and cast iron (casing, impellar and shaft)
i want to upgrade material of vertical Aerator Effluent Pump
i am thinking about nonmetallic material or steel lined...
Ladies and Gentlmen
we have corrosion problem with pump used for treated water in industrial area
material of wet pump is carbon steel and cast iron (casing, impellar and shaft)
i want to upgrade material of vertical Aerator Effluent Pump
i am thinking about nonmetallic material or steel...
Gents
Hastealloy C276 handling sulfuric acid concentration is 98% but may be diluted due to leak of NRV at Ambient temperature (4C t0 50 C), the line cracked at welded joint at HAZ
My question is how to avoid failure in HAZ in Hastealloy C276 handling sulfuric acid at ambient temperature
Hi Gents
I am Facing problem with handling sulfuric acid 98% (may be diluted) at ambient temperature (from 4C t0 50C), what is the best nonmetallic material to be used for pipes one inch and two inches