  1. JSBCintl

    20crmnti vs 8620

    We have a customer purchasing investment cast valve for recip pump valves in 8620, case hardened to 55-60Rc and wants to consider Chinese 20CrMnTi instead, to the same specs. Does anyone have experience with this material. How does it compare? Recommendations? JSBC International, Inc.
  2. JSBCintl

    8620 Steel Carburized

    I received an investment casting, suppose to be 8620 steel, case hardened to 60Rc. The chemical analysis showed the material to be as follows: C = .40 Si = .3 Mn = .65 P = .014 S = .010 Cr - .86 Mo - <.01 Ni - .04 Fe = Remainder Can someone tell me what this material might be? regards and...
  3. JSBCintl

    How does SAE 1020 compared to 20CrMoTi

    I have placed an order in China for a forging in 1020 steel. The Chinese supplier has offered to make the samples in what he calls: 20CrMoTi since the samples are only a small quantity. Once approved, they will by a production run of 1020 or Chinese #20 steel. What is 20CrMoTi steel and how...
  4. JSBCintl

    What is ASTM 620 Material

    I have a drawing of that calls out the following material. Can someone explain to me in English what this material is? In German: Din En 10139 - OC04 + LC - MA - RM Beschichlung: Din 50962 - Fe/ZnFe 0.5-3 A Disp In English: ASTM: A620; JIS G3141 SPCEN Coating Din 50962 - Fe/ZnFe 0.5 - 3 A Disp...
  5. JSBCintl

    Forging Surface finish - 1020 Steel

    What standard or normal surface finish can be expected of a 1020 Steel forging of a simple shape. See attached drawing. Also, what dimensional tolerance could be expected, ie -+ .XXX etc.
  6. JSBCintl

    Lost Wax Investment Castings

    What is the difference between silicon and water glass in an investment casting. The water glass method seems to be much cheaper and poorer surface finish. Secondly, what is the the Investment cast process that yields the best surface finish and closest to "near net shape" . The parts are...
  7. JSBCintl

    Forging

    What are the typical tolerances achieved, as forged, on a round, 6.5in dia. round part, when forged in 1020 steel. See drawing for final tolerances.
  8. JSBCintl

    what is material 8620

    This material is urethane coated and used for a valve in a mud pump, but what is the material when all they call out is Material: 8620 ??
  9. JSBCintl

    Mueller 360 Brass

    Meuller 360 Brass: Can someone tell me what this brass is and is it special in anyway, ie, costly, etc.
  10. JSBCintl

    Describe Aluminum 6061 and T numbers

    Could someone give me a simple description of AL 6061 and the significance of the T numbers and if I'm buying it in a machined state, what to watch for or be careful of. I am attempting to supply customers this metal in a machined state in various shapes,i.e. flats, rounds, shapes. Thanks for...
  11. JSBCintl

    Steel 1144 FRP

    I have a specification for Steel 1144 FRP 280-330 BHN, for use in making a Pinion Blank. Can somebody enlighten me as to the use and properties of this steel. Any help would be appreciated. JSBCintl