  1. InspCool

    3" + Process Pipe Socket welded

    Gentlemen, Has there ever occurred the use of socket welded pipe over 2" for the use of process pipe (non-utility)? I have never seen it. The custom is that, as is stated in all piping specifications, the use of socket welded pipe is reserved for auxillary, small bore, clean, non-corrosive...
  2. InspCool

    P1 to P8 carbon side cracking

    Hello, We have been attempting to perform a WPQ for P1 to P8 using ER 309 (GTAW)process. Twice now we have experienced cracking on the carbon steel side of the face bends. Is this an issue with pre-heat? Currently we do not pre-heat and I have seen qualified procedures that do not cite this as...
  3. InspCool

    DUPLICATE NAMEPLATES

    Hello, What are the rules regarding the owner installing a duplicate (replacement) nameplate on a PV? They have the U-1A form and original facsimile of the nameplate. Original manufacturer is now out of business. Internal inspection and external inspection performed and find...
  4. InspCool

    Pass partition plate hole

    My first post, glad to be a part of the group! Question: How many times have you seen a drilled hole in a pass partition plate. Can you point to a code or standard that cites why this is there. It is a perfectly centered 1/8” hole, apparently purposely drilled. I have seen this before and...