I want to harden an 1144 shaft spline to 32-38 Rc. The shaft spline is 0.875 diameter and 2.12 inches long at the end of a 16.00in. ling shaft.
Using available charts, I specified induction harden at 1500 deg F with oil quench and draw (temper) at 900 deg F for 1 hour. Does this sound OK?
I...