Guys
Working on a project which involves SUBSEA structures with duplex stainless steel (probably API 5LC LC65-2205) cooling loops within them. Inlet temperature is about 100 Celsius, although some "headroom" might be advisable.
Need to spec. amn anti-corrosion coating for the loops (which...
Guys
Working on a project which involves SUBSEA structures with duplex stainless steel (probably API 5LC LC65-2205) cooling loops within them.
Inlet temperature is about 100 Celsius, although some "headroom" might be advisable. Need to spec. amn anti-corrosion coating for the loops (which...
Working on a pipeline coated with 2.5 mm 3-layer polypropylene (nothing outstanding about it).
Using RP-F103 Table A.1 and a 3-layer FBE/PP coating I get:
a=0.1x10E-2
b=0.003*10E-2
giving
fcm = a +0.5*b*T = 0.1x10E-2 + (0.5*0.003x10E-2*25)
fcm = 0.001375
and
fcf = a + b*T
fcf = 0.1x10E-2 +...