We recently welded a specimen for procedure qualification for a SA-335 P91 to SA-335 P22 procedure. The procedure was performed on 6" Sch. 160 pipe with ER90S-B3 root and E9018-B3. Sample was PWHT at 1350F for 2 hr. Ramps were between 500F and 600F above 600F. The Tensile specimens came back as...