    Time + temp for aluminum 6082 in T0 state

    Dear colleagues, How should I anneal aluminum alloy 6082 to T0 state? I have T6 a 6082 plate (200 mm thick) and I am used to do T4 + straigthening + T6 but need T0 for forging. 540ºC + 6 hours + cooling in air would be enough? Thanks!
  2. gariartola

    Aluminum AW-4046 Preparation of the melt & casting

    Dear colleagues, I am melting an equivalent to aluminum alloy AW-4046 (9-11%Si; 0,2-0,5%Mg) and casting it into investment casting shells for a trial in the upcoming weeks and I have never dealt with this alloy. Since it is a Si-Mg alloy, I have considered to use the same amount of eutectic...