  1. rockey1

    Incorrect Nickel Plating Thickness

    Hi. My company has recently started silver plating aluminium and after microsectioning a batch of work pieces we have found that the nickel plating layer we have set down before the silver is coming out at a maximum of 16% above our maximum theoretical tollerance. So. I have set about trying...