  1. UconnMaterials

    Austempered Ductile Iron

    Hello, We have a batch of austempered ductile iron, but the cross-section doesn't look like ausferrite. This image is at 1000x and the etchant is suoer picral. Could this be bainite? The hardness is 27-29 HRC. It's also brittle as heck; I don't need to cut samples instead I just use a vice...
  2. UconnMaterials

    How Relevant is Graduate School Experience for a Position in Industry?

    I have a year left in my Materials Engineering PhD program. Recently, I started looking for a job after graduation. Fundamental research doesn't appeal to me; I would rather be doing design and development type work or materials support jobs such as failure analysis. I had 2+ years of experience...
  3. UconnMaterials

    Are Point-Contact Tests Appropriate For Testing Galling Resistance?

    Hello, I am aware of the ASTM test for galling, but many researchers use point-contact type tests for galling studies. Is this appropriate? I would expect an artificially higher galling load. For example see: Wiklund, I. M. Hutchings, Investigation of surface treatments for galling protection...