Hi guys,
I'm working as coating engineer and I have a question regarding the FBE tail protruding from a 3L-PP or 3L-PE anticorrosion coating on pipes.
In my opinion any residual FBE at the cutback area should be avoided as it could be detrimental for field joint coating and AUT operations...
Hi guys,
I'm working as coating engineer and I have a question regarding the FBE tail protruding from a 3L-PP or 3L-PE anticorrosion coating on pipes.
In my opinion any residual FBE at the cutback area should be avoided as it could be detrimental for field joint coating and AUT operations...
Hi Everybody,
I am a materials engineer and I work as coating engineer for oil & gas industry.
I was attenting a qualification test for solid polyurethane infill material for field joint coating and I experimented a quite strange behaviour of the material.
After filling the mould around the...
Hi everybody,
I'm a materials engineer and I'm working as coating engineer for an oil company. I was monitoring a PQT some days ago and I saw something quite strange so I would like to ask your opinion.
The pqt was for polyurethane infill for field joint. After filling the field joint the...