  1. SirCallipygous

    Welding A-286 and 17-4 PH

    Hi everyone. I could use some input on fusion welding A-286 thin-walled tube (.054-.065") to 17-4 PH. From what I read, the A-286 should be welded in the solution annealed condition with no post-welding heat treatment. I'm worried this won't be strong enough for my purposes (how much...