  1. edgedislocation

    why do we make grinding(stoning) before annealing?

    In my firm 304 ss wires(about 330 micron thickness) is annealed before grinding. What is the metallurgical story of annealing before grinding?(annealing is made at 650 C)
  2. edgedislocation

    Electropolishing of 316 L

    is there a better solution then phosphoric acid+sulfuric acid+lactic acid for electropolishing of 316L?
  3. edgedislocation

    TTT and CCT graphs for 316L

    are there any source for TTT and CCT graphs of 316L?
  4. edgedislocation

    The hardest polycarbonate?

    What is the hardest polycarbonate, and what is it's hardness in rockwell m and rockwell r.in addition i cant find a conversion table for rockwell r and rockwell m. I'll be so glad if i can get a conversion table about rockwell r and m.
  5. edgedislocation

    normalisation annealing 304 stainless steel

    does anyone know the 304 stainless steels normalization annealing temperature and annealing tine for a wire about 12 micron
  6. edgedislocation

    316 L annealing

    i need detailed information about annealing of 316 L which is used in stent production. If there are micrographs for different anneling temperatures i will be more pleased..