Hi
J would like to incorporate HNBR to steel by injection mold.The best way for production will be cover glue on the steel by spray and join with rubber.
Does anybodody has experience with joining steel metal with HNBR rubber?
Which glue J should choose?
J need material which could be resistant for two media :
1) 50 % NAOH solutions and tem. 140 C
2) steam water 175 C
J check Low price FKM and EPDM but with bad results.
Has anybody any idea how dissolve this problem?
regards
Miki
Good morning everybody
J'm interested in selection of material for seals which will control air flow to a diesel engine.
Temeperature range of the gasket: Temperature range = -40 ºC to +170 ºC
Maximum internal pressure (Pi) = 3.2 bar absolute.
Pressure range across the seal = -0.275 bar to +2.2...